Answer:
The formation of cracks is inherent in the nature of the raw material quartzite when the silicon linings are done.
They are contractions and volume changes involving breakage of the lining.
What can happen?
The vertical cracks, normally they close.
What to do?
1- Ideally working in 3 shifts and the furnace does not cool.
2- To observe the closing of the cracks putting the furnace back on track.
Etxerre Kaminoa 21
48970 Basauri, Vizcaya
Spain
Tel.:+34 944 409 420 (Furnaces)
Tel.:+34 944 409 450 (Refractories)
Email: insertec@insertec.biz
Fondo Europeo de Desarrollo Regional
Una manera de hacer Europa
Proyectos cofinanciados por el Programa HAZITEK – Programa de ayudas de apoyo a la I+D Empresarial del Gobierno Vasco y la Unión Europea a través del Fondo Europeo de Desarrollo Regional 2014 – 2020 (FEDER)
"NEUTRALIDAD CLIMÁTICA DE LA INDUSTRIA DEL ACERO BASADA EN NUEVAS TECNOLOGÍAS Y PROCESOS CON APLICACIÓN INTENSIVA DEL HIDRÓGENO" - H-ACERO (Expediente: ZE-2021/00025)
"NUEVAS MASAS SECAS REFRACTARIAS DE ALTO RENDIMIENTO PARA TECNOLOGÍAS DE FUNDICIÓN MEDIANTE HIC" - MASHIC (Expediente: ZL-2023/00080)
“TECNOLOGÍAS AVANZADAS PARA REPARACIONES ALTAMENTE EFICIENTES DE HORNOS HIC EN CALIENTE” - RepHIC - (Expediente: ZL-2023/0025)
"EQUIPO DE ALTA EFICIENCIA ENERGÉTICA PARA EL RECICLADO DE ALUMINIO EN BASE A TECNOLOGÍAS LIMPIAS" - RECIALEF (Expediente: ZL-2022/00049)
Esta entidad ha recibido una ayuda para la ejecución del proyecto NEXTSTEEL (CPP2021-008415), financiado por MCIN/AEI/10.13039/501100011033 y por la Unión Europea-NextGenerationEU/PRTR
© 2021 INSERTEC. All rights reserved.