Answer:
There is no single answer. There are several possible reasons that we can number as being responsible for the appearance of these cracks:
- Lining compaction inappropriate
- Segregation of the lining
- Loss of thin through the coil
- Hanging of the lining from the pan
What can happen?
Most likely metal infiltration and as a result the furnace should be demolished immediately.
What to do?
Analyse how it has been possible that it has been formed together with the supplier of the lining.
Etxerre Kaminoa 21
48970 Basauri, Vizcaya
Spain
Tel.:+34 944 409 420 (Furnaces)
Tel.:+34 944 409 450 (Refractories)
Email: insertec@insertec.biz
Fondo Europeo de Desarrollo Regional
Una manera de hacer Europa
Proyectos cofinanciados por el Programa HAZITEK – Programa de ayudas de apoyo a la I+D Empresarial del Gobierno Vasco y la Unión Europea a través del Fondo Europeo de Desarrollo Regional 2014 – 2020 (FEDER)
"NEUTRALIDAD CLIMÁTICA DE LA INDUSTRIA DEL ACERO BASADA EN NUEVAS TECNOLOGÍAS Y PROCESOS CON APLICACIÓN INTENSIVA DEL HIDRÓGENO" - H-ACERO (Expediente: ZE-2021/00025)
"NUEVAS MASAS SECAS REFRACTARIAS DE ALTO RENDIMIENTO PARA TECNOLOGÍAS DE FUNDICIÓN MEDIANTE HIC" - MASHIC (Expediente: ZL-2023/00080)
“TECNOLOGÍAS AVANZADAS PARA REPARACIONES ALTAMENTE EFICIENTES DE HORNOS HIC EN CALIENTE” - RepHIC - (Expediente: ZL-2023/0025)
"EQUIPO DE ALTA EFICIENCIA ENERGÉTICA PARA EL RECICLADO DE ALUMINIO EN BASE A TECNOLOGÍAS LIMPIAS" - RECIALEF (Expediente: ZL-2022/00049)
Esta entidad ha recibido una ayuda para la ejecución del proyecto NEXTSTEEL (CPP2021-008415), financiado por MCIN/AEI/10.13039/501100011033 y por la Unión Europea-NextGenerationEU/PRTR
© 2021 INSERTEC. All rights reserved.