Characteristics:


 - Dry silica mass based on  high puriity microcrystalline quartzite mixed with Boron Oxide (B2O3) - AN as sintering agent.


- It may also be delivered without any sintering agent.




Application:


- Lining of high medium and low frequency coreless induction furnaces melting grey or nodular iron, non


- Ferrous metals and steel casting.

Inicia sesión o regístrate para descargar la ficha técnica

Inicie sesión o regístrese para ver el precio y comprar

  • Insertec Technical Data Sheet
    Humidity We guarantee a maximun content of 0.2% at the end of the manufaturing process. Due to the different situation of transport, storage and atmosphere conditions, the moisture content could change when used. Therefore, check the moisture content in the produc
    Caracteristicas Dry silica mass based on high purity microcrystalline quartzite mixed with Boron Oxide (B2O3) - AN as sintering agent. It may also be delivered without any sintering agent.
    Application Lining of high, medium and low frecuency coreless induction furnaces melting grey or nodular iron, non-ferrous metals and steel casting.
    Temperature 1.580ºC
    Grain Size Distribution 0-7 mm
    Tipo de Ligante Boron Oxide (H2BO3) 0,8% .Find attached the Technical Data Sheet
    Chemical Analysis Al2O3 - Max.0,9%, SiO2 - (98-99)%; Fe2O3 - Máx.0,4%
    Density 2.050 - 2.200 Kg/m3
    Installation Dry hand ramming or using special vibration equipments for bottom and sidewalls. See intruction manual
    Storage Pallet must be stored in a dry place. Once opened , the pallet must be totally consumed or , at least covered with a plastic bag sheet. Maximun life of the material: 12 month
    Packing Pallet
    Drying and Heating Depending of furnaces
    Water Required Casting and Vibrating Depending on furnace´s capacity , heat up to working temperature at a rate of 100-180 ºC/h (if boron oxide binder. Sintering should be done 30-35ºC higher than working temperature , maintaining it for 0,5 - hours. See instructions manual